Our website is an independent, advertising-supported platform. We provide our content free of charge to our readers, and to keep it that way, we rely on revenue generated through advertisements and affiliate partnerships. This means that when you click on certain links on our site and make a purchase, we may earn a commission. Learn more.
How We Make Money
We sustain our operations through affiliate commissions and advertising. If you click on an affiliate link and make a purchase, we may receive a commission from the merchant at no additional cost to you. We also display advertisements on our website, which help generate revenue to support our work and keep our content free for readers. Our editorial team operates independently of our advertising and affiliate partnerships to ensure that our content remains unbiased and focused on providing you with the best information and recommendations based on thorough research and honest evaluations. To remain transparent, we’ve provided a list of our current affiliate partners here.

What is a Welding Procedure Specification?

By Larry Ray Palmer
Updated May 17, 2024
Our promise to you
About Mechanics is dedicated to creating trustworthy, high-quality content that always prioritizes transparency, integrity, and inclusivity above all else. Our ensure that our content creation and review process includes rigorous fact-checking, evidence-based, and continual updates to ensure accuracy and reliability.

Our Promise to you

Founded in 2002, our company has been a trusted resource for readers seeking informative and engaging content. Our dedication to quality remains unwavering—and will never change. We follow a strict editorial policy, ensuring that our content is authored by highly qualified professionals and edited by subject matter experts. This guarantees that everything we publish is objective, accurate, and trustworthy.

Over the years, we've refined our approach to cover a wide range of topics, providing readers with reliable and practical advice to enhance their knowledge and skills. That's why millions of readers turn to us each year. Join us in celebrating the joy of learning, guided by standards you can trust.

Editorial Standards

At About Mechanics, we are committed to creating content that you can trust. Our editorial process is designed to ensure that every piece of content we publish is accurate, reliable, and informative.

Our team of experienced writers and editors follows a strict set of guidelines to ensure the highest quality content. We conduct thorough research, fact-check all information, and rely on credible sources to back up our claims. Our content is reviewed by subject-matter experts to ensure accuracy and clarity.

We believe in transparency and maintain editorial independence from our advertisers. Our team does not receive direct compensation from advertisers, allowing us to create unbiased content that prioritizes your interests.

A welding procedure specification (WPS) is an outline of the specific welding procedures and techniques that can be used with specific metals and metal alloys. Using the WPS sheet, a properly trained welder can replicate the same results every time. The specification is determined using a test weld that is recorded in the procedure qualification record (PQR). The use of these specifications is mandated by several major industrial organizations.

The welding procedure specification is a product of safety and production standards. It is used to outline what welding procedures can be used to create safe and durable welds with a given material. This outline ensures consumer safety and the uniformity of building and production codes. Prior to employment, welders are required to be tested on their understanding of the specifications of the metals and processes they will be working with, and this test is recorded in the welder qualification test record (WQTR).

A variety of information for a given metal type and the welding process that can be used with the metal is included in a welding procedure specification. In the most basic form, the specification sheet provides the procedure number and process type of the test weld, followed by the pertinent information needed to duplicate the test result. Also included in the description is other information, such as the thickness and type of metal being welded, the welding procedures and process types used for the test welds, the fuel types or electrical current used in the welding process, the use or lack of preheating, the applicable welding codes and other variables. In cases when the weld is critical to the structure, more detailed specifications — such as the assembly order of the joint, required heat treatments and arc energy limits — are provided to ensure the creation of a solid weld.

In addition to the basic information regarding the welding processes and the metals used, the welding procedure specification should also include sketches of the weld and the joint set-up process prior to welding. The production sequence might also be included if it is integral to how the weld is made. By following all of this information, any competent welder should be able to achieve the same effects as the test welder.

The WPS records the best welding practice for a given metal or alloy, but it does not cover nondestructive testing. Separate nondestructive testing processes are required. This nondestructive testing procedure is also recorded, but it generally is not included in the welding procedure specification.

About Mechanics is dedicated to providing accurate and trustworthy information. We carefully select reputable sources and employ a rigorous fact-checking process to maintain the highest standards. To learn more about our commitment to accuracy, read our editorial process.
Discussion Comments
About Mechanics, in your inbox

Our latest articles, guides, and more, delivered daily.

About Mechanics, in your inbox

Our latest articles, guides, and more, delivered daily.